Copper Nickel Alloy Low Finned Tube ASME SB111 UNS C70600 CuNi 90/10 For Shell Tube Heat Exhanger

Categories Fin Tube
Brand Name: YUHONG
Model Number: ASTM B111 UNS C70600 Copper Alloy Low finned Tube
Certification: ABS, GL, DNV, NK, PED, AD2000, GOST9941-81, CCS, ISO 9001-2008
Place of Origin: China
MOQ: 500 KGS
Price: Negotiable
Payment Terms: L/C,T/T
Supply Ability: 800 Tons/ month
Delivery Time: 7 DAYS
Packaging Details: Ply-wooden Case /Iron Case/ Bundle with plastic Cap etc.
Main Tube Size: OD: 15.88-63.5mm , Thk.1.65-4.57mm
Tube W.T.: 1.65-4.57mm
Fin Thickness: 0.2mm~3.0mm
Fin Height: 1.6mm ~60mm
End: Plain End, Beveled End
Application: Shell Tube Heat Exhanger
Company Info.
Yuhong Group Co.,Ltd
Verified Supplier
View Contact Details
Product List
  • Haven't found right suppliers
  • Our buyer assistants can help you find the most suitable, 100% reliable suppliers from China.
  • And this service is free of charge.
  • we have buyer assistants who speak English, French, Spanish......and we are ready to help you anytime!
Submit Buying Request
  • Product Details
  • Company Profile

Copper Nickel Alloy Low Finned Tube ASME SB111 UNS C70600 CuNi 90/10 For Shell Tube Heat Exhanger

Copper Nickel Alloy Low Finned Tube ASME SB111 UNS C70600 CuNi 90/10 For Shell Tube Heat Exhanger


This specification ASTM B111 establishes requirements for copper and various copper alloys seamless tubing and tubing tubing in a specified range of diameters for use in surface condensers, evaporators, and heat exchangers. The copper and copper alloys specified are UNS Nos. C10100, C10200, C10300, C10800, C12000, C12200, C14200, C19200, C23000, C28000, C44300, C44400, C44500, C60800, C61300, C61400, C68700, C70400, C70600, C70620, C71000, C71500, C71520, C71640, and C72200.The products shall be produced by casting, extruding, drawing, annealing, straightening, and trimming, and by any other process which will produce seamless tubes under specified conditions.


Copper and copper alloys shall be supplied in any of the following hardened states: annealed, lightly drawn, hard drawn or hard drawn and finally annealed. Tubing for ferrules shall be fully annealed to full crystallization. Stress relieving heat treatment is recommended for certain tubing after straightening.


Products should be tested for expansion, compression and residual stress. Tensile and expansion requirements for the product are specified according to the steel grade designation. Products shall also be subjected to mercury nitrite test, ammonia vapor test, eddy current test, hydrostatic test and pneumatic test.


Material


GradeUSAU.KGermanyJapan
China BGASTM B 111BSDINJIS H
BFe10-1-1C70600CN102CuNi10Fe1MnC7060

Standards and Composition


Trade NameUNSCopper Nickel Industry SpecificationsChemical CompositionMin. Tensile
(KSI)
Min. Yield
(KSI)
Elongation
%
CuNi 90/10UNS C70600
UNS C70620
ASME SB111, SB171, SB359, SB395, SB466, SB467, SB543
ASTM B111, B122, B151, B171, B359, B395, B432, B466, B467, B543, B608 DIN 2.0872 MIL C-15726, T-15005, T-16420, T-22214 SAE J461, J463
Cu 88.6 min
Pb. 05 max*
Fe 1.8 max
Zn
1 max*
Ni 9-11 max
Mn 1.0 max
381530
CuNi 90/10UNS C70600EEMUA 144 90/10, 145 90/10, 14 90/1Cu rem.
Pb. 01 max
Fe 1.5-2.0
Zn 0.2 max
P 0.2 max
S 0.2 max
Ni 10-11
Mn 0.5-1.0
401530
CuNi 70/30UNS C71500
UNS C71520
ASME SB111, SB171, SB359, SB395, SB466, SB467, SB543
ASTM B111, B122, B151, B171, B359, B395, B432, B467, B543, B552, B608, F467, F468
DIN 2.0882
MIL C-15726, T-15005, T-16420, T-22214
SAE J461, J463
Cu rem (65.0 min)
Pb. 05 max*
Fe 0.4-1.0
Zn 1 max*
Ni 29-33
Mn 1 max
521845
CuNi 70/30UNS C71640ASTM B111, B543, B552Cu rem
Pb. 05 max*
Fe 1.7-2.3
Zn 1 max*
Ni 29-32
Mn 1.5-2.5
6325


Standard Dimensions - Low Finned Tubes
Outside DiameterThicknessLengthFin Density
(mm)(inch)(mm)(BWG)(m)(ft)(fins/inch)(fins/m)
12.00~ 60.000.47~ 2.40.635 ~ 4.57223 ~ 70.3 ~ 251 ~ 828 ~ 40315 ~ 1575

Materials - Low Finned Tubes
Carbon SteelSA 179 / A 179
Carbon SteelSA 210 / A 210
Carbon SteelSA 334 / A 334
Stainless SteelSA 213 / A 213
Duplex Stainless SteelSA 789 / A 789
Copper & Cu AlloysSB 111 / B 111
Titanium & Ti AlloysSB 338 / B 338
For different materials please contact our sales department.
Standard Technical Specifications - Low Finned Tubes
Carbon SteelASTM A 498
Stainless SteelASTM A 1012
Copper and Copper AlloysASTM B 359
TitaniumASTM B 891
For different materials please contact our sales department.

ALSO AVAILABLE - LOW FINNED TUBES
Condenser Tube "Y-fin"Evaporator Tube "T-fin"
Inner Grooved (IG) Low Fin TubeInner Grooved (IG) Y-Fin / T-fin Tube
U-Bent Low Fin TubeAnnealed Low Fin Tube
Inspections and Tests - Low Finned Tubes
Chemical Composition
Mechanical Properties
Hydrostatic Test
Pneumatic Test
Boroscopic Inspection
Eddy Current Test

Quality Copper Nickel Alloy Low Finned Tube ASME SB111 UNS C70600 CuNi 90/10 For Shell Tube Heat Exhanger for sale
Send your message to this supplier
 
*From:
*To: Yuhong Group Co.,Ltd
*Subject:
*Message:
Characters Remaining: (0/3000)
 
Inquiry Cart 0