| Brand Name: | PANGANGGROUP,TISCO,ANSTEEL,BAOSTEEL |
| Model Number: | Udimet 710, ATG W4 |
| Certification: | SGS, TUV, BV, ISO, MTC |
| Place of Origin: | China |
| MOQ: | 600kg |
| Price: | Negotiations |
| Payment Terms: | T/T |
| Supply Ability: | 50000KGS/Month |
| Delivery Time: | Ex-stock for delivery: 3-7 days Production lead time: 30-60 days |
| Packaging Details: | Wooden Pallet BOX;Standard Seaworthy Package;based on the customer's special requirement |
| Product Name: | Udimet 710, ATG W4 Superalloy |
| Characteristic: | Anti-oxidation, Creep resistance |
| Heat treatment condition: | +P, +NT, etc |
| Processing methods: | Machined, etc |
| Available Shapes: | Steel plate, Sheet, Coil, etc |
| Surface: | Rrough Turned, Centreless Ground, etc |
Udimet 710 Superalloy Sheet Steel ATG W4 Hot Rolled Strips
Product Information
Udimet 710 superalloy has good oxidation resistance and creep resistance, and can be strengthened by precipitation hardening, solution hardening and work hardening. They also function under high mechanical stress and high temperature and where high surface stability is required
Size Range
Round bar / Wire rod (Diameter): 1.0 mm to 500 mm
Square bar / Flat bar: 1.0 mm to 500 mm
Forging piece: Stepped shafts with flanks / discs /tubes /slugs
/donuts /cubes /other different shapes based on OEM.
Heavy/middle plate via hot rolled: T3 - 1000 mm X W8 - 1000 mm X
L800-12000 mm
Sheet steel via cold rolled: T5.0 - 8 mm X W5 - 1000 mm X L100 -
1000 mm
Steel strip via cold rolled: T0.3 - 8 mm X W10 - 1000 mm X L (or in
coil form)
Length: Fixed length or random length or based on the customer's
special requirement.
Chemical Composition and standard
| ATG W4 |
ASTM A959(2004) | JIS G4303(2005) |
W(%): ≤1.50 Al(%): ≤2.50 Ti(%): ≤5.0 Fe(%): ≤0.50 Co(%): ≤14.8 B(%): ≤0.02 | C(%): ≤0.07 W(%): ≤1.50 Al(%): ≤2.50 Ti(%): ≤5.0 Fe(%): - Co(%): - B(%): ≤0.02 |

X120Mn12/1.3401 Mechanical Properties
Tensile strength, Rm/MPa: -
Yield strength, Rp/MPa: -
Elongation/%: -
Reduction of area, ψ/%: --
Impact, KV /J: -
Hardness, HBW: --
Applications
Udimet 710 is suitable for various high-temperature environments, such as steam and gas turbines.