| Sign In | Join Free | My carsrow.com |
|
| Categories | EP Rubber Conveyor Belt |
|---|---|
| MOQ: | 100 |
| Price: | 23-30 |
| Payment Terms: | T/T |
| Supply Ability: | 30000m/month |
| Delivery Time: | 7-14 days |
| Packaging Details: | 200 m per roll or customized request |
| Brand Name: | Toptempo |
| Model Number: | EP800/4(6+2)*1600 |
| Place of Origin: | Qingdao,China |
| Material: | rubber |
| Conveyor belt thickness: | 4-20mm |
| Belt width: | 400-2200mm |
| Cover rubber grade: | DIN 22102 RMA,AS1332,etc... |
| Tensile strength: | 15-25Mpa |
| Company Info. |
| TOPTEMPO INDUSTRIAL CO.,LTD |
| View Contact Details |
| Product List |
Product features: Heat resistant EP conveyor belt
| Standards | Cover Rubber | Adhesion | ||||
| Tensile Strength | Elongation at break | Abrasion | Cover to Ply | Cover to Ply | Ply to Ply | |
| DIN 22102 | Mpa | % | mm3 | N/mm | N/mm | N/mm |
| DIN 22102-Z | 15 | 350 | 250 | 3.5 | 4.5 | 5 |
| DIN 22102-W | 18 | 400 | 90 | 3.5 | 4.5 | 5 |
| DIN 22102-Y | 20 | 400 | 150 | 3.5 | 4.5 | 5 |
| DIN 22102-X | 25 | 450 | 120 | 3.5 | 4.5 | 5 |
| Standards | Cover Rubber | Adhesion | ||||
| Tensile Strength | Elongation at break | Abrasion | Cover to Ply | Cover to Ply | Ply to Ply | |
| AS 1332 | Mpa | % | mm3 | N/mm | N/mm | N/mm |
| AS 1332-N | 17 | 400 | 200 | 4 | 4.8 | 6 |
| AS 1332-M | 24 | 450 | 125 | 4 | 4.8 | 6 |
| AS 1332-E | 14 | 300 | | 4 | 4.8 | 6 |
| AS 1332-A | 17 | 400 | 70 | 4 | 4.8 | 6 |
| Standards | Cover Rubber | Adhesion | ||||
| Tensile Strength | Elongation at break | Abrasion | Cover to Ply | Cover to Ply | Ply to Ply | |
| RMA | Mpa | % | mm3 | N/mm | N/mm | N/mm |
| RMA-I | 17 | 400 | | 3 | 4.4 | 4 |
| RMA-II | 14 | 400 | | 3 | 4.4 | 4 |
· Polyester conveyor belt, also called EP or PN conveyor belt, whose tension resistant body is canvas woven by polyester in warp and polyamide in weft.
· The belt has the characteristics of low elongation in warp and good trough ability in weft, good water resistance, good wet strength, suitable for medium, long distance and heavy-load transportation of materials.
· Because of the high initial modulus of polyester, the belts can choose a relative low safety factor.

| Carcass | Fabric structure | Type | No. of plies | Cover thickness | Belt width | ||
| Warp | Weft | Top | Bottom | ||||
| EP | Polyester | Nylon-66 | EP80 | 2-6 | 3.0-18.0 | 1.5-10.0 | 300-5000 |
| EP100 | |||||||
| EP125 | |||||||
| EP150 | |||||||
| EP200 | |||||||
| EP250 | |||||||
| EP300 | |||||||
| EP350 | |||||||
| EP400 | |||||||
| EP500 | |||||||
Physical property indexes
| Item | Type | |||
| 1 | 2 | 3 | ||
| Range | ||||
| Hardness | Difference before and after aging (IRHD) | 20 | ±20 | |
| Maximum value after aging (IRHD) | 85 | |||
| Tensile Strength | Change rate of property % ≤ | 25 | 30 | 40 |
| Minimum value after aging /Mpa | 12 | 10 | 5 | |
| Breaking Elongation | Change rate of property % ≤ | 50 | 55 | |
| Minimum value after aging % | 200 | 180 | ||
|