| Sign In | Join Free | My carsrow.com |
|
| Categories | Vacuum Sintering Furnace |
|---|---|
| Brand Name: | EasyFashion Industry |
| Model Number: | GN5518A |
| Certification: | CE Certificate |
| Place of Origin: | China |
| MOQ: | 1 set |
| Supply Ability: | 10 set per year |
| Delivery Time: | 120 days |
| Packaging Details: | Standard packed by wooden cases and container. |
| Ultimate vacuum: | ≤2Pa, tested in cold and clean chamber |
| Dimension of furnace: | 4500×5400×3500 mm |
| Dimension of usable space: | 500×500×1800 mm |
| Max. load weight: | 1500 kg |
| Wax collecting rate: | ≥98﹪ |
| Stand area: | ≈5200×6000 mm |
Main Description
Integrated Vacuum Degreasing and Sintering Furnace integrate the functions of de-waxing, sintering, atmosphere controlling and cooling etc.
Technical specifications
Model | GN5518A | GN3312A |
Rated voltage | 380 V 50 Hz, three-phase five-wire | |
Dimension of usable space | 500×500×1800 mm | 300×300×1200mm |
Dimension of furnace | 4500×5400×3500 mm | 4500×4250×3500 mm |
Max. load weight | 1500 kg | 500 kg |
Weight of furnace | ≈5500 kg | ≈4000 kg |
Stand area | ≈5200×6000 mm | ≈4500×4000mm |
Power | 340 kVA | 200 kVA |
Max. testing temperature | 1600°C | |
Max. working temperature | ≤1550°C | |
Temperature control method | 3 zones | |
Ultimate vacuum | ≤2Pa, tested in cold and clean chamber | |
Pumping speed (in cold and clean chamber) | ≤20 min., pumping from 1.13×105Pa to 5Pa | |
Com deviation | ≤±0.2% | |
Temperature increasing rate (without loading) | 15°C/min(≤1000℃); 10°C/min(≥1000℃) | |
Temperature uniformity | ≤±7°C (Ceramic ring) | |
Vacuum Leak rate | ≤2Pa/h(24 hours average), tested in cold and clean chamber | |
Hc deviation | ≤±0.3KA/M | |
Wax collecting rate | ≥98﹪ | |
Cooling speed (without loading) (cooling water ≤30°C) | From working temp. to 800°C, ≤ 3 h From 800°C to opening door, ≤ 6 h | From working temp. to 800°C, ≤ 2 h From 800°C to opening door, ≤ 5 h |
|