Brand Name: Torich
Model Number: Alloy Steel Pipe HastelloyX
Certification: CE PED
Place of Origin: China
MOQ: 1000kg
Price: negotiable
Payment Terms: L/C, T/T
Supply Ability: 200 tons per year
Delivery Time: 6-8 weeks
Packaging Details: In bundles in woode box
Similar Grade: GH3536, GH536,GH22, GH334, GH739, SG-5, UNS N06002, NC22FeD, NiCr22FeMo, Nimonic PE13
Material: Hastelloy C
Application: Used in the manufacture of aircraft engine combustion chamber components and other high temperature components
Density: 8.28g/cm³
Melting temperature: 1295℃-1381℃
  • Haven't found right suppliers
  • Our buyer assistants can help you find the most suitable, 100% reliable suppliers from China.
  • And this service is free of charge.
  • we have buyer assistants who speak English, French, Spanish......and we are ready to help you anytime!
Submit Buying Request
  • Product Details
  • Company Profile

Aircraft Engine Hastelloy X Alloy Steel Pipe Nickel Based Superalloy With Iron

Alloy Steel Pipe HastelloyX


Hastelloy X is a kind of nickel-based superalloy with high iron content, which is mainly solution strengthened by chromium and molybdenum solution strengthening. It has good resistance to oxidation and corrosion resistance. It has good cold & hot formability and weldability because its moderate lasting and creep strength under 900℃. Used in the manufacture of aircraft engine combustion chamber components and other high temperature components. It can be long-term used under 900℃, and short-term working temperature can up to 1080℃.


Similar Grade of Hastelloy X: GH3536, GH536,GH22, GH334, GH739, SG-5, UNS N06002, NC22FeD, NiCr22FeMo, Nimonic PE13, Hastelloy H


Application for Hastelloy X: Used in the manufacture of aircraft engine combustion chamber components and other high temperature components


Chemical Composition of Hastelloy X:


Chemical Composition (%)
CCrNiCoWMoAlTiFeBCuMnSiPS
0.05-0.1520.5-23.0Margin0.50-2.500.20-1.00

8.0-

10.0

≤0.50≤0.1517.0-20.0≤0.010≤0.5≤1.00≤1.00≤0.025≤0.015

Hastelloy X Physical Properties:


Hastelloy X Density: ρ: 8.28g/cm³


Hastelloy X Melting Temperature Rage: 1295℃-1381℃


Coefficient of Thermal Conductivity of Hastelloy X:


coefficient of thermal conductivity
Temperature
100200300400500600700800900
λ/(w/(m.℃))13.3817.9720.2722.424.6226.7929.0531.14

33.44


Specific Heat Capacity for Hastelloy X:


Specific Heat Capacity
Temperature
17100200300400500600700800900
C/J/( kg · K )372.6372.6389.4456.4427.1452.2464.7515535.9561

Expansion Coefficient for Hastelloy X:


expansion coefficient
Temperature/℃20-10020-20020-30020-40020-50020-60020-70020-80020-900
α1/10-6℃-112.112.513.41414.314.815.515.816.1

Resistivity of Hastelloy X:


resistivity
Temperature/℃100200300400500600700800900
Resistor
Ω·m
1.181.21.211.221.241.251.261.271.29

Hastelloy X is widely used in aircraft engine and the civilian industry in adroad, and in our country, it mainly used in the manufacture of hot end of combustion chamber parts and other components, and honeycomb structure, etc. Besides, long-term used at high temperature will have certain age hardening phenomenon.





Quality Aircraft Engine Hastelloy X Alloy Steel Pipe Nickel Based Superalloy With Iron for sale
Send your message to this supplier
 
*From:
*To: TORICH INTERNATIONAL LIMITED
*Subject:
*Message:
Characters Remaining: (0/3000)
 
Inquiry Cart 0